Setter Plates

From 650 °C to 1700 °C: choose the plate by your temperature, atmosphere and product.

A setter plate is where your product stands in the kiln. If the plate cracks, the product is scrapped with it. If the plate reacts with the product, parts stick or discolor. MLCC, zirconia and LTCC each ask for something different: flatness and strength, permeability for binder burnout, or no reaction with the product.

Start from your problem

Our three general-purpose grades are all corundum-mullite. Each is built to solve one problem. Which one carries more load depends on your product weight and temperature, so tell us both.

Plates bend or sag
76C
Built to resist deformation at high temperature. Our first recommendation for load-bearing setters and posts.
Plates crack
86C-3
Built for thermal shock: fast heating and cooling, many cycles. Test it in your kiln first. Also the only grade we supply as a pusher plate.
Product gets scratched
86C-7
Fine grain and a smooth surface, so parts are not scratched as they shrink. The trade-off is the lowest deformation resistance of the three.

Where both 76C and 86C-3 suit your conditions, one can stand in for the other, so supply does not depend on a single grade.

Choose a grade by firing conditions

GradeTypeTemperatureSuited toNote
76CCorundum-mullite (Al₂O₃ approx. 79%), resists high-temperature deformationMax. 1700 °CWhere plates tend to bend: load-bearing setters, postsCracks more easily than 86C-3 under fast heating and cooling
86C-3Corundum-mullite (approx. 86%), resists thermal shockUp to 1700 °C long-term as a setterWhere plates tend to crack. As a pusher plate: approx. 1400 °C long-termLess deformation resistance than 76C. On large plates with big temperature differences, assess expansion slots
86C-7Corundum-mullite (approx. 86%), fine grain, smooth surface, high flexural strengthMax. 1700 °CAlumina green tape, small zirconia parts. Zirconia-coated: MLCC base plate. Footed version availableUncoated plates cannot be used in reducing atmospheres
99-Z199.5% alumina, developed for HTCCMax. 1600 °CHTCC sintering: high purity, smooth surface, porosity that helps debinding. Also strong thin platesNot available in large sizes
99DK99% high-porosity alumina plate, porosity approx. 70%Max. 1700 °CMLCC, LTCC, HTCC and zirconia that need gas permeability and no contaminationNot load-bearing: use as an underlay. Liquids soak in
99-299% alumina tile with higher porosityUsed at approx. 1380 °CMetal parts and MIM in pusher kilnsAbove 100 × 100 mm it is cut from a larger plate
1300HSMachinable high-strength board, no dusting1200 °C long-termLTCC debinding and sintering, glass bending molds, traysThe heating curve depends on your process
Zirconia-coated setter plateComposite: zirconia outer layer on an alumina-based plateUsed at approx. 1300 °CMLCC and other products that need a barrier against reaction and stickingCoating thickness to order

Temperatures are typical values and describe the material at near-zero load. With product on the plate the usable temperature is lower, so please tell us your load. Open-lattice porous setters (max. 1550 °C) have their own page.

Typical values of the three general grades

Property76C86C-386C-7
Al₂O₃ (%)78.986.786.9
SiO₂ (%)20.412.612.4
Bulk density (g/cm³)2.672.912.85
Apparent porosity (%)17.212.813.5
Flexural strength (MPa)15.513.622.8
Thermal conductivity (W/m·K)2.12.32.3
Maximum service temperature (°C)170017001700

Typical values, not guaranteed values. Thermal expansion and thermal shock data are available on request. Flatness depends on size, thickness and grade, so we confirm it for each order.

Sizes we have made

In mm. The largest so far is 1000 × 500. Any of these can be made again, and other sizes to order. We recommend grade and thickness for your conditions.

1000×500 · 850×390 · 665×360 · 650×390 · 600×450 · 430×300 · 420×270 · 400×180 · 365×270 · 340×340 · 325×165 · 320×190 · 280×280 · 260×220 · 250×250 · 220×220 · 190×125 · 150×150 · 115×115 · round spacers Φ25, Φ35

Ask us for the full size list

Using setter plates

Pre-fire new plates. Fire them empty until they no longer affect the product. Once is usually enough.
Expansion slots only where needed. Assess them for large plates, large temperature differences or frequent fast cycles. Keep supports away from the slots.
Slow the heating rate after switching to a more permeable plate. Binder leaves faster, and the old curve may crack product edges.
For heavy products, choose a larger plate and add a post under the middle. Plate thickness depends on load, size and setting.

Common questions

RELATED INDUSTRIES
MLCC LTCC / HTCC Zirconia and structural ceramics Ferrite and inductors MIM Glass bending
Why do setter plates crack, and do expansion slots help?
Cracking depends on cooling rate, load, plate size, stacking height and process. Expansion slots relieve stress but cannot guarantee a crack-free plate. Before full production, run a small batch on your line.
Why does product stick to the plate? Will grinding fix it?
Sticking is usually a reaction between the plate material and the product, so it comes back after grinding. Change the material, or add a barrier layer such as a zirconia coating.
What flatness can you hold?
Flatness depends on size, thickness and grade, so there is no single figure. Send us the size and your requirement, and we confirm it for that grade.

Get a quote for setter plates

Grade, size and quantity are enough for a price. Only your email is required. We usually reply within 1–3 business days.

Not sure which grade fits? Choose "Not sure yet" and tick the box to add your firing conditions. We suggest a grade, and a sample if you want to test first.

Email: sales@youka-tech.com

PRODUCT: SETTER PLATES

Loading the form…

We use your details only to answer your inquiry. See our Privacy Policy.