Kiln Furniture for LTCC and HTCC Co-Firing

Clean binder burnout, flat substrates, no contamination.

In co-fired ceramics, many layers of green tape and printed conductors are fired together. Binder must leave every layer evenly, the stack must stay flat, and nothing from the setter may react with or stick to the substrate.

LTCC fires at low temperature, below about 1000 °C, where binder burnout is the critical step. HTCC fires at high temperature in a reducing atmosphere, where purity and flatness matter most. We supply setters for both, and help you choose by your process.

What co-fired ceramic lines care about

ConcernWhy it mattersWhat helps
Clean binder burnoutResidual carbon turns substrates dark and causes defectsPermeable setters: 99DK, porous setters, 1300HS for LTCC
Flatness and warpingThin multilayer substrates warp easily during firingFlat, ground setters; a porous setter on top as a light cover plate
Sticking and surface pitsSilver and glass phases can stick to the setterChoose the setter surface by your paste and product; ask us
PurityImpurities from the setter can react with the substrateHigh-purity alumina: 99-Z1, 99DK, porous setters (99.5% Al₂O₃)
Batch consistencyShrinkage must stay stable from lot to lotStart with a small batch and agree acceptance criteria

Setters for LTCC and HTCC

ProductWhat it isMax. service temperatureUse in co-firingNote
1300HSMachinable high-strength board, no dusting1200 °C long-termLTCC debinding and sinteringHeating curve depends on your process
99DK99% high-porosity alumina plate, approx. 70% porosity1700 °CDebinding underlay for LTCC and HTCCNot load-bearing
Porous setters G4-1 / G5-199.5% alumina, open 3D lattice1550 °CHTCC firing and debinding; light cover plate against warpingG5-1 for sensitive surfaces
99-Z199.5% alumina setter developed for HTCC1600 °CHTCC sintering: high purity, smooth surfaceNot available in large sizes

Maximum service temperatures are material properties at near-zero load. Typical values, not guaranteed values.

Questions from LTCC and HTCC lines

Our substrates warp or come out dark. Is it the setter?
Not always. Warping and darkening often start earlier in the process: tape, paste, lamination or the burnout profile. The setter can play a part, through flatness, permeability or the way the stack is supported. Send us your conditions and photos, and we check together whether the kiln furniture is part of the cause.
Which setter should we start with?
For LTCC debinding and sintering, 1300HS or a permeable plate such as 99DK. For HTCC, 99-Z1 or porous setters. Tell us your paste, temperatures and substrate size, and we suggest a starting point and a sample.
RELATED

Ask about LTCC and HTCC setters

Send the product and size for a price, or describe your process for a recommendation. Only your email is required. We usually reply within 1–3 business days, and can arrange a sample.

Send inquiry
IF YOU WANT A RECOMMENDATION, THESE HELP
  • LTCC or HTCC, and the conductor paste (silver, copper, tungsten …)
  • Burnout and peak temperatures, atmosphere
  • Substrate size, thickness and number of layers per stack
  • The setter you use now, and the problem you see