MLCC Setter Racks & Zirconia-Coated Nickel Mesh

A matched set for stacking MLCC chips in reducing-atmosphere firing.

The rack is a 99% dense alumina frame that holds the mesh and lets you stack layers in the kiln. The nickel mesh carries the chips; its zirconia coating keeps the chips from reacting with the nickel. Also called setter frames or firing jigs.

Both are in production use at several leading MLCC producers in China. We help with sizing for your kiln and loading, sample trials, and problem analysis when something goes wrong in production.

approx. 450,000
Setter racks delivered (as of October 2026)
approx. 150,000
Zirconia-coated nickel meshes delivered
99.6% Al₂O₃
Dense alumina racks (typical)
35–150 μm
Zirconia coating thickness, to order
SETTER RACK

99% dense alumina racks

PropertyTypical value
Al₂O₃99.6%
Bulk density3.89 g/cm³
Apparent porosity0.3%
Flexural strength186 MPa
Max. service temperature1400 °C
Standard sizes: square approx. 250 × 250 mm; long approx. 300 × 150 mm. Custom sizes on request; height and layer spacing are confirmed for your kiln and loading.
NICKEL MESH

Zirconia-coated nickel mesh

ItemDetail
CoatingZirconia, 35–150 μm, to order
Mesh countTo order; 32 mesh is the most common
Standard sizes270 × 140 mm and 230 × 230 mm, matched to the two rack sizes. Custom sizes on request
AtmosphereReducing or inert only. Not for use in air
TemperatureBelow approx. 1300–1400 °C
Best used on a rack. Supported only by spacers at the edges, a mesh may warp.
Buy as a set or separately. Racks and mesh come in matching standard sizes, and each can be ordered on its own.

Use them as a set

Most problems with racks and mesh come from atmosphere, support and handling rather than from the material.

Confirm the atmosphere first. Nickel mesh works only in reducing or inert atmosphere.
Put the mesh on a rack. Edge spacers alone let the mesh warp.
Pre-fire new furniture, usually once, until it no longer affects the product.
Keep racks below about 1400 °C long-term, and do not lift a rack by one corner.
A pale green mesh is normal. It is the nickel changing color and does not affect use.
Go from sample to production in steps. Heat is less even in a full kiln, so the curve may need adjusting.
WHAT WE DO NOT PROMISE
  • We do not quote a service life for the mesh. It depends on your atmosphere, temperature and handling.
  • The mesh is not for use in air or in atmospheres containing oxygen.
What we do: confirm the size and weight for your kiln before sampling, agree acceptance criteria with you, and send an inspection report with each shipment. 8D reports on request.
MLCC firing: conditions, concerns and a case

Questions about racks and mesh

Why do setter racks break?
Three common causes: the long-term temperature is too high (keep it below about 1400 °C); the rack is supported differently in use than when it was fired, so stress concentrates; or it is lifted by one corner. If racks still break, send us your kiln type, loading and photos of the break.
Why does the zirconia coating come off the mesh?
Usual causes are oxygen in the atmosphere, an uneven coating, or poor adhesion. Use the mesh only in a reducing or inert atmosphere.
Why does the mesh warp?
Most often because it is supported only at the edges. Lay the mesh on a rack so it is supported across its area.
Can the mesh be used in air?
We advise against it. In air, nickel oxidizes and expands, which pushes the zirconia coating off.
RELATED

Get a quote for racks and mesh

Tell us what you need, the size and the quantity. Only your email is required. We usually reply within 1–3 business days.

For a new line, we suggest starting with samples, then a small production batch before full volume.