Pusher Plates & Kiln Posts

Plates that carry the load through a pusher kiln, and posts that build the stack.

In a continuous pusher kiln, plates move forward one after another carrying the product. They take heavy load and friction at high temperature for a long time. Our corundum-mullite pusher plates combine good thermal shock resistance with high elastic modulus, flexural strength and creep resistance.

Kiln posts support setter plates layer by layer, so you can use the full height of the kiln. We have made posts in many sizes and make them to your drawing.

86C-3
Our pusher plate grade
approx. 1400 °C
Long-term use as a pusher plate
9 sizes
Posts made before, available again
To drawing
Plates and posts made to your kiln
PUSHER PLATES

Corundum-mullite, grade 86C-3

We supply pusher plates in one grade only. Other grades do not perform well as pusher plates. As a pusher plate, 86C-3 is used long-term at about 1400 °C. Above 1500 °C its wear resistance is not enough.

Property86C-3 typical value
Al₂O₃86.7%
SiO₂12.6%
Bulk density2.91 g/cm³
Apparent porosity12.8%
Flexural strength13.6 MPa
Thermal conductivity2.3 W/m·K
Sizes: made before: 338 × 338 × 30 mm. Other sizes made to your kiln drawing.
KILN POSTS

Posts in sizes we have made

Usually made in corundum-mullite grade 76C; 86C-3 is also available.

Size (mm)
408 × 50 × 50
408 × 50 × 30
408 × 30 × 30
350 × 50
165 × 20
75 × 75
70 × 40
20 × 20
20 × 15
All of these can be made again. Other sizes and special shapes to your drawing.

Longer life for pusher plates

Pusher plate cracking is closely linked to fast heating and cooling.

Push slowly. The slower the plates move through the temperature change, the better.
Cool slowly. Fast cooling is the most common cause of cracks.
Keep long-term use near 1400 °C. Above 1500 °C, wear increases quickly.
Tell us the load per plate. Weight and temperature together decide how a plate lasts.

No plate can be guaranteed against cracking if it goes from kiln temperature to room temperature in a short time.

Questions about pusher plates and posts

Why do our pusher plates crack?
Most often because of fast heating or cooling. Slow down the push rate and the cooling, and check that the long-term temperature stays near 1400 °C. If cracks continue, send us the kiln type, push rate, load and photos.
Can we use other setter grades as pusher plates?
We do not recommend it. Only 86C-3 performs well as a pusher plate in our range.
Can you make posts to our size?
Yes. Send us a drawing or the dimensions and the load they carry. The nine sizes above have been made before and can be made again.
RELATED

Get a quote for pusher plates and posts

Tell us the item, size and quantity. Only your email is required. We usually reply within 1–3 business days.

You can also send a drawing by email after submitting the form.

Email: sales@youka-tech.com

PRODUCT: PUSHER PLATES & KILN POSTS

Loading the form…

We use your details only to answer your inquiry. See our Privacy Policy.